Post by 1st Sail »

We will see where this goes. I'm tired of buffing and waxing the stripes etc. with little durability. On the prep side I've run the gamut using all the marine grade polishing compounds + a number of 3M marine grade grinds of compounds. Up to that point the results are pure shine. I used several of the leading marine wax/polishes with the exception of Collinite. Same results after 4-6 weeks, oxidized stripes.

This time around I'm giving New Glass a run. I called them Wed and had a great discussion with their support staff. Their recommendation is to use soft scrub for stains and polish the stripes. He stated clearly colors are the issue ie. blue hull or black stripes as both tend to oxidize at a greater rate and depth than the white. He recommended that the colors must be polished to remove the oxidation. You do not have to polish to a high gloss as New Glass will provide the gloss. It is very important to remove all oxidation as New Glass forms a chemical bond with the gel coat where as wax / polishes form a mechanical bond and therefor never alter the gelcoat on a chemical basis.

So I'm prepping the surface by washing normal dirt and stains with soap and water, wipe down. Next rinse the surface and then buff/compound with random orbital buffer until black stripe oxidation is remove and color is pure. I'm buffing with either soft scrub or 3m cutting cream. Spray on New Glass cleaner then scrub with pad/sponge. Wash with water and towel dry to remove water spots. Next wipe on 4-5 coats New Glass. Wait approximately 1-3 minutes between coats. Done.

The boat will sit outside on the trailer until mid-Oct. So I will keep you posted on oxidation levels.

FYI streaking has not been an issue as New Glass is very low viscosity. Also I wipe each coat in a different direction of travel rotating 45' between application direction. There is some shrinking of the film during drying which also provides some leveling.

The gloss on the port side so far is excellent.

There doesn't appear to be any significant color influence from New Glass after 5 coats. The white color has a very slight warm cast which I believe is primarily due to the reduction in specular reflection of the surface and actually more toward the slight warm white of the original color coat during mfg.

Fingers crossed!
Dave
User avatar
Tomfoolery
Admiral
Posts: 6135
Joined: Tue Jul 05, 2011 7:42 am
Sailboat: MacGregor 26X
Location: Rochester, NY '99X BF50 'Tomfoolery'

Re: New Glass

Post by Tomfoolery »

Pics! We (ok, I) need pics!

Mine badly needs that sort of TLC, and New Glass has made the short list. Collinite Fleetwax works very well on the hull, but the decks need much more work than I'm willing to invest, though NG sounds like it might be the ticket there.
User avatar
kelseydo
Chief Steward
Posts: 87
Joined: Sat Apr 04, 2009 9:49 am
Sailboat: MacGregor 26X
Location: Utah

Re: New Glass

Post by kelseydo »

Dave,
Great post. I too went with New Glass II on my 96X this year for the same reasons and with exactly the same results. Their service rep was very helpful and proud of their product . Time will tell.
Dan
User avatar
Erik Hardtle
First Officer
Posts: 408
Joined: Sat Jan 03, 2004 4:45 am
Sailboat: MacGregor 26X
Location: New Bern, NC
Contact:

Re: New Glass

Post by Erik Hardtle »

Here is a link to another thread about the product... I use it:

http://www.macgregorsailors.com/forum/v ... =9&t=20697

Pic!(I'm the shiny one)
Image
Post Reply